'bare metal'

It's been quite a while since I did 'real' refinishing.
Here, in the pestilential swamp, as soon as one gets down to bare metal, you're almost compelled to immediately prime and seal, or oxidation takes off and contaminates adhesion.
Hope Delaware's an improvement over North Texas.
Will you be using the epoxy primer system? I understand that it's wayyyyyyyyyyyyyy out ahead of the old DuPont system I used.