Quote:
Originally Posted by bschloop
Pete, is that 450g/m2? over here they measure mat in weight per sq ft for some reason, while cloth is per sq yd. I did play around with some 6oz cloth yesterday, and found it to be too flexible even with 4 layers. is there any good way to get a smooth outer finish on csm? or am I just going to have to do a lot of sanding and filling?
|
Exactly!!
That is why I use a thin layer of foam between only TWO layers of 6 ounce glass.
Half the weight and about 8 times the strength!
Jim.