View Single Post
Old 09-28-2016, 11:31 AM   #116 (permalink)
Macskyver
EcoModding Lurker
 
Join Date: Aug 2016
Location: Texas
Posts: 86
Thanks: 0
Thanked 225 Times in 56 Posts
Quote:
Originally Posted by freebeard View Post
I'd expect we're talking about convex (bead) and concave (cove) edges rather than tongue and groove.
Exactly. Post #40 on this thread has a good graphic showing it.


Quote:
Originally Posted by skyking View Post
The epoxy will yellow over time with exposure to the sun. I used WR-LPU from system three as a protective clear coat.
https://www.systemthree.com/products...ethane-topcoat
Yep. I got a different product, but also from system three to prevent the yellowing due to UV radiation. This is what I have:

https://www.systemthree.com/collecti...e-spar-varnish
  Reply With Quote